A "geometric model" of glass-enamel coating. Part 2. Contact area with metal, the gas-phase volume fraction, and the minimum coating's cross-section / Shardakov N.T., Kudyakov V.Ya. // Protection of Metals. - 2005. - V. 41, l. 4. - P. 411-414.

ISSN:
00331732
Type:
Article
Abstract:
In terms of a geometric model, an equation of the minimum cross-section area of a glass-enamel coating, as well as its particular form to calculate the contact area between the coating and the metal substrate, is derived. The expressions to assess the gas-phase volume fraction in the coating and its density are also obtained. It is shown that tearing the coating off occurs most probably in the plane of the minimum coating's cross-section rather than the metal/coating interface. © Pleiades Publishing, Inc.
Author keywords:
Index keywords:
Adhesion; Bubbles (in fluids); Enamels; Functions; Glass; Integral equations; Mathematical models; Volume fraction; Cohesion; Geometric models; Glass-enamel coatings (GEC); Surface areas; Enameling
DOI:
10.1007/s11124-005-0058-4
Смотреть в Scopus:
https://www.scopus.com/inward/record.uri?eid=2-s2.0-23844458241&doi=10.1007%2fs11124-005-0058-4&partnerID=40&md5=e7cc4244ff011d4669a2f734788f3795
Соавторы в МНС:
Другие поля
Поле Значение
Link https://www.scopus.com/inward/record.uri?eid=2-s2.0-23844458241&doi=10.1007%2fs11124-005-0058-4&partnerID=40&md5=e7cc4244ff011d4669a2f734788f3795
Affiliations Institute of High-Temperature Electrochemistry, Ural Division, Russian Academy of Sciences, ul. S. Kovalevskoi 20, Yekaterinburg, 620219, Russian Federation
References Shardakov, N.T., Kudyakov, V.Ya., (2004) Zashch. Met., 40 (6), p. 634
Correspondence Address Shardakov, N.T.; Institute of High-Temperature Electrochemistry, Ural Division, Russian Academy of Sciences, ul. S. Kovalevskoi 20, Yekaterinburg, 620219, Russian Federation
Language of Original Document English
Abbreviated Source Title Prot. Met.
Source Scopus