EFFECT OF OXIDES RO, R2O3, RO2 AND IMPURITY MATERIALS ON DECOMPOSITION DURING HEATING OF KYANITE IN OXIDIZING AND REDUCING ATMOSPHERES / Kashcheev I. D.,Sychev S. N.,Elizarov A. Yu. // REFRACTORIES AND INDUSTRIAL CERAMICS. - 2011. - V. 52, l. 1. - P. 44-47.

ISSN/EISSN:
1083-4877 / нет данных
Type:
Article
Abstract:
The effect of impurity minerals and oxides RO, R2O3 and RO2 (R-II = Mg, Ca, R-III = Fe, Cr, R-IV = Ti, Zr) on thermal decomposition parameters for kyanite concentrate of the Karabash deposit, linear expansion of composition with continuous heating, physicomechanical properties and change in specimen phase composition, are studied.
Author keywords:
kyanite; mullite; cristobalite; impurities; linear expansion
DOI:
нет данных
Web of Science ID:
ISI:000291490300011
Соавторы в МНС:
Другие поля
Поле Значение
Month MAY
Publisher CONSULTANTS BUREAU/SPRINGER
Address 233 SPRING ST, NEW YORK, NY 10013 USA
Language English
Research-Areas Materials Science
Web-of-Science-Categories Materials Science, Ceramics
ResearcherID-Numbers Elizarov, Andrei/C-2560-2014 Kashcheev, Ivan/O-1809-2015
ORCID-Numbers Elizarov, Andrei/0000-0001-6846-1282 Kashcheev, Ivan/0000-0003-0153-5974
Number-of-Cited-References 5
Usage-Count-Since-2013 2
Journal-ISO Refract. Ind. Ceram.
Doc-Delivery-Number 775VA