Silicon carbide refractory castables / Kamenskikh VA,Kashcheev ID,Mityushov NA,Gulyaev AA,Kotova MV,Kiselev AS,Leshkeev SA // REFRACTORIES AND INDUSTRIAL CERAMICS. - 2005. - V. 46, l. 6. - P. 412-415.

ISSN/EISSN:
1083-4877 / нет данных
Type:
Article
Abstract:
Optimum formulations for castables intended for different service conditions are proposed. Silicon carbide castables containing ultradisperse particles of cement, silica fume, and electrofused corundum are developed. The castables do not weaken on heating and display superior operational properties: the compressive strength is 40 - 80 MPa at sintering temperature 400 degrees C and 50 - 85 MPa at 1300 degrees C, the strain onset temperature under a load of 0.2 MPa is 1700 - 1510 degrees C; thermal stability (1300 degrees C - water) is better than 45 heating/cooling cycles (1300 degrees C- water); no change in linear and volume dimensions was observed on heating. The newly-developed castables can find application in various sectors of industry, in particular, as the refractory material for the lining of Whiting furnaces and porcelain kilns.
Author keywords:
нет данных
DOI:
10.1007/s11148-006-0037-6
Web of Science ID:
ISI:000237823600009
Соавторы в МНС:
Другие поля
Поле Значение
Month NOV-DEC
Publisher CONSULTANTS BUREAU/SPRINGER
Address 233 SPRING ST, NEW YORK, NY 10013 USA
Language English
Research-Areas Materials Science
Web-of-Science-Categories Materials Science, Ceramics
ResearcherID-Numbers Kashcheev, Ivan/O-1809-2015
ORCID-Numbers Kashcheev, Ivan/0000-0003-0153-5974
Number-of-Cited-References 2
Usage-Count-Since-2013 1
Journal-ISO Refract. Ind. Ceram.
Doc-Delivery-Number 046PN