Features of reduction of high-magnesia nickel ore of the serov deposit / Selivanov E. N.,Sergeeva S. V.,Udoeva L. Yu. // RUSSIAN JOURNAL OF NON-FERROUS METALS. - 2010. - V. 51, l. 6. - P. 439-442.

ISSN/EISSN:
1067-8212 / нет данных
Type:
Article
Abstract:
Parameters of reducing the roasting of high-magnesia oxide nickel ore containing, wt \%, 1.2 Ni, 0.026 Co, 17.0 Fe(2)O(3), 4.0 Al(2)O(3), 20.2 MgO, and 46.0 SiO(2) are evaluated. The degrees of reduction and metallization upon heating the ore with the reducing agent in the range t = 800-1250A degrees C and the sizes of metallic inclusions forming in the course of the process are determined. To separate the phases, the magnetic separation of reducing products at H = 40 and 80 kA/m is used. The best characteristics are attained upon roasting the ore with a reducing agent and a sulfidizing agent at t = 1300A degrees C. In this case, the magnetic fraction contains 7.1\% Ni, while the nonmagnetic one contains 0.18\% Ni.
Author keywords:
nickel ore; reduction; magnetic separation; roasting; recovery
DOI:
10.3103/S1067821210060015
Web of Science ID:
ISI:000285975400001
Соавторы в МНС:
Другие поля
Поле Значение
Month DEC
Publisher ALLERTON PRESS INC
Address 18 WEST 27TH ST, NEW YORK, NY 10001 USA
Language English
Research-Areas Metallurgy \& Metallurgical Engineering
Web-of-Science-Categories Metallurgy \& Metallurgical Engineering
Author-Email pcmlab@mail.ru lyuud@yandex.ru
ResearcherID-Numbers Selivanov, Evgeniy/T-7296-2017
Number-of-Cited-References 8
Usage-Count-Last-180-days 1
Usage-Count-Since-2013 4
Journal-ISO Russ. J. Non-Ferrous Metals
Doc-Delivery-Number 703JY